SURFACTANT LEACHING:
Concentration of water-soluble ingredients on water-based paint, creating a blotchy, sometimes glossy appearance, often with a tan or brownish cast. More likely with tinted paints than with white or factory-coloured paints.

POSSIBLE CAUSES:
• Painting in cool, humid conditions or just before they occur. The longer drying time allows the paint's water-soluble ingredients - which would normally evaporate, or be leached out by rain or dew - to rise to the surface before paint thoroughly dries.

• Mist, dew or other moisture drying on the painted surface shortly after it has dried.

SOLUTION:
• If possible, avoid painting in the late afternoon if cool, damp conditions are expected in the evening or overnight. If the problem occurs in the first day or so after the paint is applied, the water-soluble material can sometimes be rinsed off rather easily. Fortunately, even more stubborn cases will generally weather off in a month or so. Surfactant leaching should not affect the ultimate durability of the coating.

< Back

PQI Brazil
Home | Legal Disclaimer | Privacy Statement | Photo Credits
© 2001-2008 Paint Quality Institute - All rights
PQI China PQI France PQI Germany PQI Russia PQI South Africa PQI Schweden PQI USA PQI Brazil PQI  Australia/New Zealand