FOAMING / CRATERING:
Formation of bubbles (foaming) and resulting small, round concave depressions (cratering) when bubbles break in a paint film, during paint application and drying.

POSSIBLE CAUSES:
• Shaking a partially filled can of paint.

• Use of low quality paint or very old water-based paints.

• Applying (especially rolling) paint too rapidly.

• Use of a roller cover with wrong nap length.

• Excessive rolling or brushing of the paint.

• Applying a gloss or satin paint over a porous surface.

SOLUTION:
• All paints will foam to some degree during application; however, higher quality paints are formulated so the bubbles break while the paint is still wet, allowing for good flow and appearance. Avoid excessive rolling or brushing of the paint or using paint that is more than a year old. Apply gloss and satin paints with a short nap roller, and apply an appropriate sealer or primer before using such paint over a porous surface. Problem areas should be sanded before repainting.

< Back

PQI Brazil
Home | Legal Disclaimer | Privacy Statement | Photo Credits
© 2001-2008 Paint Quality Institute - All rights
PQI China PQI France PQI Germany PQI Russia PQI South Africa PQI Schweden PQI USA PQI Brazil PQI  Australia/New Zealand